Properties

GOHSENOL™ EG series is Polyvinyl Alcohol obtained through purification process. Production facility, production management, and quality assurance all meet the criteria of self-imposed standards of GMP for pharmaceutical excipients.

Grades List

GOHSENOL™ EG granule type

Grades Degree of hydrolysis[mol%] Viscosity *1, *2 (Unit of measurement)[mm2/s]
EG-03P 86.5-89.0 3.0-3.8 (3.4)
EG-05P 4.5-6.1 (5.3)
EG-18P 15.3-20.7 (18.0)
EG-22P 19.0-25.6 (22.3)
EG-30P 25.5-34.5 (30.0)
EG-40P 36.6-49.4 (43.0)
EG-48P 41.3-55.7 (48.5)
*1: 4%solution, under 20 deg. C
*2: indicated as JPE value. Viscosity specifications fulfilling requirements of other pharmacopoeia are available upon request

GOHSENOL™ EG powder type

Grades Degree of hydrolysis[mol%] Viscosity *1, *2 (Unit of measurement)[mm2/s]
EG-05PW 86.5-89.0 4.5-6.1 (5.3)
EG-30PW 25.5-34.5 (30.0)
EG-40PW 36.6-49.4 (43.0)
*1: 4%solution, under 20 deg. C
*2: indicated as JPE value. Viscosity specifications fulfilling requirements of other pharmacopoeia are available upon request

Applications

Binder, Film coating agent, Thickener (for ophthalmic, nasal solutions), Gel patch, Emulsifier, OD film substrate.

Dissolution and Storage

Dissolving GOHSENOL™ EG

GOHSENOL™ EG is charged into room temperature water slowly in small amounts while stirring to disperse. The water is heated, and with constant stirring, kept at 80 to 90 degree C for 30 to 60 minutes.

Storing GOHSENOL™ EG

Avoid storage in tanks or pipes that readily rust.

Comparison of Effluent Water Loads of Water Soluble Polymer
Polymer COD(mg/l) BOD5(mg/l)
GOHSENOL™ EG-40 89 180
Corn Starch 36 7400
Measuring conditions: Sample concentrations mean pure material concentrations.
COD was measured by potassium permanganate method (JIS K 0102), and BOD5 means the BOD value of over 5 days.